Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ASTM D792 |
PolyOne Maxxam™ FR PP 402 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ISO 1183 |
Polimeri Europa Clearflex® FG 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FG 106 are characterized by .. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ASTM D792 |
PolyOne Versaflex™ OM 1040X-1 Thermoplastic Elastomer (TPE) The Versaflex™ OM 1040X-1 is a medical compliant overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, A.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ISO 1183 |
Polimeri Europa Flexirene® CL 10 U Butene Copolymer Linear Low Density Polyethylene Flexirene CL 10 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexi.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ISO 1183 |
Polimeri Europa Flexirene® FG 20 F Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 F is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 F is recommended for the .. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ISO 1183 |
Polimeri Europa Riblene® MQ 10 Low Density Polyethylene - Injection Molding Riblene MQ 10 is a good fluidity low density polyethylene resin (LDPE).Parts made with Riblene MQ 10 are characterized by a high flexibility.Main Applications: Riblene MQ 10 is suitable for injecti.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ISO 1183 |
Polimeri Europa Riblene® MR 10 R Low Density Polyethylene - Injection Molding Riblene MR 10 R is a high fluidity low density polyethylene resin (LDPE).Parts made with Riblene MR 10 R are characterized by a high flexibility.Main Applications: Riblene MR 10 R is suitable for i.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ASTM D792 |
PolyOne Dynaflex™ G7430-9001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7430-9001-00 is an easy processing, high performance compound designed for use in applications requiring tough, durable material. - Excellent Heat Stability - Good Ozone and UV Stability.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ASTM D792 |
PolyOne Dynaflex™ G7431-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7431-1001-00 is an easy processing, performance TPE designed for use in applications requiring a tough, durable material with a low coefficient of friction. - Excellent Heat Stability - .. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ASTM D792 |
PolyOne Maxxam™ FR MF5420-0013 FR Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ISO 1183 |
Polimeri Europa Clearflex® FF 106 Hexene Copolymer Linear Low Density Polyethylene Clearflex FF 106 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Clearflex FF 106 are characterized by .. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ISO 1183 |
Polimeri Europa Flexirene® CL 10 Butene Copolymer Linear Low Density Polyethylene Flexirene CL 10 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for cast extrusion of thin film with high optical properties.Main Applications: Flexire.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ISO 1183 |
Polimeri Europa Flexirene® FG 20 I Butene Copolymer Linear Low Density Polyethylene Flexirene FG 20 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 I is recommended for the .. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ASTM D1505 |
LG Chemical LUTENE LB4500 LDPE Extrusion Coating Description: LUTENE LB4500 is mainly intended for extrusion coating and can be processed uniform thickness and width. LUTENE LB4500 is also noted for the excellent heat stability and has good silico.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ASTM D1505 |
LG Chemical LUTENE LB5000 LDPE Extrusion Coating Description: LUTENE LB5000 is mainly intended for extrusion coating and can be processed at high speed uniform thickness and width. LUTENE LB5000 is also noted for the excellent adhesion to porous a.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ASTM D792 |
Spartech SP-1310 Polyolefin Sheet Description: Polyolefin SheetInformation provided by Spartech. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ASTM D792 |
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ISO 1183 |
Total LDPE 1070 MN 18 C Low Density Polyethylene - Injection Molding and Compounding LDPE 1070 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant. Grade adapted to the production of flexible parts with a high production rate.Applicat.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ISO 1183 |
Total LDPE 1700 MN 18 C Low Density Polyethylene - Injection Molding and Compounding LDPE 1700 MN 18 C is a low density polyethylene made by a high pressure autoclave process without antioxidant. Grade for easy flow injection molding of flexible parts, powder production for grindin.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ISO 1183 |
Total Lotrene® Q2018H Linear Low Density Polyethylene, Blown Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ASTM D792 |
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ASTM D792 |
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ASTM D792 |
Total Lotrene® Q1018H Linear Low Density Polyethylene, Blown Film Lotrene® Q1018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for blown film applications and can be used in pure.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ISO 1183 |
Total Lotrene® Q2018N Linear Low Density Polyethylene, Cast Film Lotrene® Q2018 Series are Linear Low Density Polyethylene resins produced in a gas phase reactor using butene (C4) co-monomer. They are designed for film applications and can be used in pure form .. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ASTM D1505/D792 |
Braskem BC818 Extrusion Coating Low Density Polyethylene Description: BC818 is a grade produced under high pressure in an autoclave reactor. In the coating process it presents very good optical properties, low neck-in, good film stability, and good adhesi.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ASTM D1505/D792 |
Braskem Green PE SLL318 Blow Film Extrusion and Cast Film Extrusion Linear Low Density Polyethylene Description: SLL118 is a Linear Low Density Polyethylene, copolymer of butene-1. Developed for blown film extrusion in blends with polyethylenes. Films obtained with this product show a good process.. |
|||
Specific Gravity | 0.918 g/cc | 0.918 g/cc | ASTM D1505/D792 |
Braskem LL218 Cast Film Extrusion Linear Low Density Polyethylene Stretch films; Liners; LDPE and HDPE blends; Packages for general use.Information provided by Braskem. |
|||
Specific Gravity | 0.918 - 0.922 g/cc | 0.918 - 0.922 g/cc | ASTM D1505 |
LG Chemical SEETEC SF316 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Additives- Medium slip agent, Medium antiblocking agentApplications: Agricultural & i.. |
|||
Specific Gravity | 0.918 - 0.922 g/cc | 0.918 - 0.922 g/cc | ASTM D1505 |
LG Chemical SEETEC SF318 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati.. |
|||
Specific Gravity | 0.918 - 0.922 g/cc | 0.918 - 0.922 g/cc | ASTM D1505 |
LG Chemical SEETEC SN318 Linear Low Density Polyethylene, Blown Film Grade Features: Characteristics- Good tensile & tear strength, High clarity, mechanical strength & sealing properties. Comonomer: Octene-1. Additives- Medium slip agent, Medium antiblocking agentApplicati.. |