Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.820 g/cc | 0.820 g/cc | |
Parker Chomerics CHO-BOND® 1087 Primer Description: CHO-BOND® 1087 Primer is a low viscosity, blue liquid formulated to provide adhesion between silicone based compounds and non-silicone substrates such as metal, glass, plastic and cera.. |
|||
Specific Gravity | 0.820 - 0.840 g/cc | 0.820 - 0.840 g/cc | |
Michelman® Topaz Indicator 17 Solution Description: Primer for use with HP Indigo press s2000Usage: Topaz 17 Solution is a solvent based primer designed to be applied via screen printing on plastic sheets to make them print compatible wi.. |
|||
Specific Gravity | 0.820 g/cc | 0.820 g/cc | |
Momentive Performance Materials SS4120 Silicone Primer for use with RTV Silicone Adhesive Sealants, Clear SS4004P, SS4044P, SS4120, SS4155, and SS4179 primers are formulated for use with GE Silicones RTV silicone rubber adhesive sealants. GE Silicones one-component products offer primerless adhesion.. |
|||
Specific Gravity | 0.820 g/cc | 0.820 g/cc | |
Momentive Performance Materials SS4155 Silicone Primer for use with RTV Silicone Adhesive Sealants, Blue SS4004P, SS4044P, SS4120, SS4155, and SS4179 primers are formulated for use with GE Silicones RTV silicone rubber adhesive sealants. GE Silicones one-component products offer primerless adhesion.. |
|||
Specific Gravity | 0.820 g/cc | 0.820 g/cc | |
Shin-Etsu Silicones MK80 Fluid Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Specific Gravity | 0.820 g/cc | 0.820 g/cc | 15°C; ASTM D1298 |
ExxonMobil Gargoyle Arctic 224 SHC 200 Series Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt.. |
|||
Specific Gravity | 0.820 g/cc @Temperature 25.0 °C |
0.820 g/cc @Temperature 77.0 °F |
|
Dow Corning HV 1860/120 PRIMER Primer designed for use with peroxide curing silicone rubbers to provide good bonding to metal, glass fibre and epoxy resinInformation provided by Dow Corning |
|||
Specific Gravity | 0.820 g/cc @Temperature 25.0 °C |
0.820 g/cc @Temperature 77.0 °F |
|
Dow Corning OS-20 Information provided by Dow Corning |
|||
Specific Gravity | 0.820 g/cc @Temperature 25.0 °C |
0.820 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPPMX-200 1CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 1CS. A polydimethylsiloxane polymer for use in skincare, suncare, woundcare, hair care, and color cosmetic applications. INCI Name: TrisiloxaneInf.. |
|||
Specific Gravity | 0.820 g/cc @Temperature 25.0 °C |
0.820 g/cc @Temperature 77.0 °F |
|
Dow Corning 200® 1 CST FLUID A polydimethylsiloxane polymer for use in skincare, suncare, woundcare, hair care, and color cosmetic applications.Information provided by Dow Corning |
|||
Specific Gravity | 0.820 g/cc | 0.820 g/cc | 15°C; ASTM D1298 |
ExxonMobil Gargoyle Arctic 224 SHC 200 Series Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt.. |
|||
Specific Gravity | 0.820 g/cc | 0.820 g/cc | |
BCC Products HPX-850 Epoxy Backfill System HPX-850 is a light weight, heat resistant, two component epoxy backfill system. HPX-850 features advantages such as low cost, long pot life, machineability, and low shrinkage. HPX-850 is ideally su.. |