Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.770 g/cc @Temperature 25.0 °C |
0.770 g/cc @Temperature 77.0 °F |
|
Dow Corning OS-120 Information provided by Dow Corning |
|||
Specific Gravity | 0.770 g/cc @Temperature 25.0 °C |
0.770 g/cc @Temperature 77.0 °F |
|
Dow Corning Z-6079 SILANE DOW CORNING Z6079 Silane is useful in protecting OH and SH functionality of complex molecules, permitting other sites to be selectively reacted.Information provided by Dow Corning |
|||
Specific Gravity | 0.770 g/cc | 0.770 g/cc | ASTM-D-792-66 |
BCC Products MB 3500 Urethane Fixture Board MB 3500 is an extremely tough, high impact Urethane Plank, that can replace aluminum and other metals for many foundry applications. Features: excellent machinability, low dust emission, mostly sha.. |
|||
Specific Gravity | 0.770 g/cc | 0.770 g/cc | ASTM D3574 |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Specific Gravity | 0.770 - 0.800 g/cc | 0.770 - 0.800 g/cc | |
Kraton® NEXAR™ MD9150 Polymer Barrier Membrane Solution NEXAR™ sulfonated block copolymer membranes are designed for water transport, filtration and separation. They have a high moisture vapor transportation rate, allowing usage in humidification and d.. |