Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.620 - 0.650 g/cc | 0.620 - 0.650 g/cc | 15.6/15.6°C; ASTM D287 |
LG Chemical IP-40 Structure & Characteristics: C5H10. A ring-structured saturated hydrocarbon. Present in naphtha pyrolysis oil and is obtained by distillation followed by isolation of n-pentane extraction remnants o.. |
|||
Specific Gravity | 0.620 - 0.650 g/cc | 0.620 - 0.650 g/cc | 15.6/15.6°C; ASTM D225 |
LG Chemical i-Pentane Structure & Characteristics: C5H10. A ring-structured saturated hydrocarbon. Present in naphtha pyrolysis oil and is obtained by distillation followed by isolation of n-pentane extraction remnants o.. |
|||
Specific Gravity | 0.620 - 0.650 g/cc | 0.620 - 0.650 g/cc | 15.6/15.6°C; ASTM D287 |
LG Chemical n-Pentane CH3CH2CH3. Saturated hydrocarbon fatty acid. Dissolved in crude oil. Colorless gas with slightly characteristic odor, and is heavier than air.Uses: Used as an EPS foaming agent named 'styrofoam' by .. |