Polymer Property : Specific Gravity = 0.600 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.600 g/cc
0.600 g/cc
Mixed; TM R050-16
Resinlab® EP1287 Filled, Flame Retardant Epoxy Syntactic Foam
Resinlab™ EP1287 is a two part filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-extinguishin..
Specific Gravity 0.600 - 0.800 g/cc
0.600 - 0.800 g/cc
Gromax Paraformaldehyde 9%
Information provided by Gromax Enterprises Corp.
Specific Gravity 0.600 g/cc
0.600 g/cc
Apparent
Shin-Etsu Silicones KSP-102 Fluid
Information Provided by Shin-Etsu Silicones of America, Inc.
Specific Gravity 0.600 - 0.700 g/cc
0.600 - 0.700 g/cc
ASTM D-792
Axiall 3802 Vinyl Foam, Extrusion
Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall..