Polymer Property : Brookfield Viscosity = 750000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 750000 - 2.20e+6 cP

@Temperature 25.0 °C
750000 - 2.20e+6 cP

@Temperature 77.0 °F
380NS Resin; HBF, Helipath, 5rpm, T-bar Spindle E
Lord Adhesives Fusor® 380NS / 383NS Epoxy Adhesive
LORD Fusor® 380NS/383NS adhesive is a two-part, rapid-cure epoxy adhesive used to bond fiberglass reinforced plastics (FRP), sheet molded compounds (SMC) and metals.All information provided by Lo..