Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 390 cP @Temperature 25.0 °C |
390 cP @Temperature 77.0 °F |
9929B; ASTM D2369-87; LVT |
Lord Adhesives Aeroglaze® 9929 Epoxy Primer Aeroglaze® 9929 epoxy primer is designed to be used on properly prepared aluminum and steel surfaces for applications that require protection against corrosion.All information provided by Lord. |