Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 88.9 cm | 35.0 in | |
PolyOne Geon™ Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Spiral Flow | 88.9 cm | 35.0 in | |
PolyOne Geon™ Vinyl Rigid Molding M4885 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Spiral Flow | 88.9 cm | 35.0 in | |
PolyOne Geon™ Vinyl Rigid Molding M5700 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Spiral Flow | 88.9 cm | 35.0 in | |
PolyOne Geon™ Vinyl Rigid Molding M5705 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Spiral Flow | 88.9 cm | 35.0 in | |
PolyOne Geon™ Vinyl Rigid Molding M5730 Natural Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of.. |
|||
Spiral Flow | 88.9 cm | 35.0 in | |
PolyOne Geon™ Vinyl Rigid Molding M5731 Polyvinyl Chloride, Rigid (PVC, Rigid) NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. Dark colored compounds do not.. |
|||
Spiral Flow | 88.9 cm | 35.0 in | |
PolyOne Geon™ 80510 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Spiral Flow | 88.9 cm | 35.0 in | |
PolyOne Geon™ 83510 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Spiral Flow | 88.9 cm | 35.0 in | |
PolyOne Geon™ Vinyl Rigid Molding M4820 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |