Polymer Property : Spiral Flow = 26.0 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 66.0 cm
26.0 in
PolyOne Geon™ Vinyl Rigid Molding MR201 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Spiral Flow 66.0 cm
26.0 in
PolyOne Geon™ Vinyl Rigid Molding MR900 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Spiral Flow 66.0 cm
26.0 in
PolyOne Geon™ 80530 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Spiral Flow 66.0 - 90.0 cm
26.0 - 35.4 in
177°C/1000 psi
Cookson Group Plaskon® 2929BNSC Epoxy Molding Compound  (discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound for the encapsulation of semiconductor devices and fiber optics. Excellent moldability (good release, ..
Spiral Flow 66.0 - 664 cm
26.0 - 261 in
Average value: 129 cm Grade Count:11
Overview of materials for Nylon 66, 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. ..
Spiral Flow 66.0 cm
26.0 in
Cross Section: 7[mm]x3.5[mm]; AKRO
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..