Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.027 - 0.031 cm/cm @Time 86400 sec |
0.027 - 0.031 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp KX99792 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KX99792 is a compound based on Acetal Copolymer resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the .. |
|||
Linear Mold Shrinkage, Flow | 0.027 - 0.031 cm/cm @Time 86400 sec |
0.027 - 0.031 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp KX99792 Acetal Copolymer LNP* Lubricomp* KX99792 is a compound based on Acetal Copolymer resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the .. |
|||
Linear Mold Shrinkage, Flow | 0.027 - 0.031 cm/cm | 0.027 - 0.031 in/in | ASTM D955 |
PolyOne Geon™ Vinyl Flexible A55G0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |