Polymer Property : Linear Mold Shrinkage, Flow = 0.0220 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0220 cm/cm

@Thickness 3.17 mm
0.0220 in/in

@Thickness 0.125 in
ASTM D955
Oxford Polymers C-Acetal 10MF-900 BK Acetal
Product Description: Acetal Injection Molding Grade, 10 melt flow Processing and Delivery Form: Pellets and Injection MoldingSpecial Characteristics: Pre-colored blackInformation provided by Oxford..