Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0139 cm/cm @Thickness 2.00 mm |
0.0139 in/in @Thickness 0.0787 in |
TPE Method |
SCG Chemicals EL-Proâ„¢ P740J Polypropylene Injection Molding Key Characteristics:Good flowabilityGood processabilityHigh stiffnessRecommended Applications:Automotive, motorcycle and electrical appliance parts that require good flowability such as automotive t.. |