Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0135 - 0.0165 cm/cm | 0.0135 - 0.0165 in/in | |
LATI Latene® 7 TR-V2 PP Homopolymer, Mineral Reinforced, Flame Retardant Polypropylene homopolymer (PPh) based compound. Mineral filler. UL94 V-2 classified, with brominated flame retardants, PBB/PBDE free. Good surface appearance.Availability: Africa & Middle East; Asia.. |
|||
Linear Mold Shrinkage, Flow | 0.0135 - 0.0165 cm/cm | 0.0135 - 0.0165 in/in | |
LATI Latene® EP 7-V2HF PP Copolymer, Flame Retardant Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; N.. |
|||
Linear Mold Shrinkage, Flow | 0.0135 - 0.015 cm/cm | 0.0135 - 0.015 in/in | ISO DIS 294-4 |
Wellman Wellamid® GS1684-WBK1 25% Glass Sphere Filled Nylon 66 Description: Glass Sphere Filled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Flow | 0.0135 cm/cm | 0.0135 in/in | |
BASF Procom® X25H 650 Polypropylene Electrical and domestic appliances, housings where high gloss is required.Data was collected by ISO methods and provided by BASF. |