Polymer Property : Linear Mold Shrinkage, Flow = 0.0122 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0122 cm/cm
0.0122 in/in
60x60x2mm; ISO 294
BASF Ultradur B 4300 G2 10% Glass Filled PBT
Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
Linear Mold Shrinkage, Flow 0.0122 cm/cm
0.0122 in/in
ISO 2577
BASF Ultradur® B 4300 G2 FC 10% Glass Filled PBT
Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulation..