Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0092 - 0.0094 cm/cm @Time 86400 sec |
0.0092 - 0.0094 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Thermocomp OB008 PPS - Branched LNP* Thermocomp* OB008 is a compound based on Branched PPS containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0088 - 0.0094 cm/cm @Thickness 3.20 mm |
0.0088 - 0.0094 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Linear Mold Shrinkage, Flow | 0.0088 - 0.0094 cm/cm @Thickness 3.20 mm |
0.0088 - 0.0094 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Asia Pacific) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |
|||
Linear Mold Shrinkage, Flow | 0.0088 - 0.0094 cm/cm @Thickness 3.20 mm |
0.0088 - 0.0094 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL GTX GTX4610 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX4610 resin is a high performance, 10% glass filled blend of PPE/PA that exhibits an excellent balance of non-halogenated flame retardance, dimensional stability, high heat resistance, .. |