Polymer Property : Linear Mold Shrinkage, Flow = 0.00800 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00400 - 0.00800 cm/cm
0.00400 - 0.00800 in/in
Compression; ISO 2577
Raschig Group 4554 Silicone
Glass fiber reinforced silicone molding compound. Excellent thermal stability - up to 300°C, exceptional electrical properties, good mechanical strength, very good dimensional stability. Processi..
Linear Mold Shrinkage, Flow 0.00600 - 0.00800 cm/cm
0.00600 - 0.00800 in/in
Injection; ISO 2577
Raschig Group DECAL® 1760 Phenolic
Glass-fiber reinforced phenolic molding compound. Very good electrical properties, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals an..
Linear Mold Shrinkage, Flow 0.00600 - 0.00800 cm/cm
0.00600 - 0.00800 in/in
Injection and Compression; ISO 2577
Raschig Group DECAL® 5431 Phenolic
Organically and inorganically filled phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/..