Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0050 - 0.0078 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0078 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0078 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0078 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0078 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0078 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® SLX1432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0078 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0078 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0078 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0078 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0050 - 0.0078 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0078 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® SLX2432D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East reg.. |