Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00500 - 0.00700 cm/cm

@Thickness 3.17 mm
0.00500 - 0.00700 in/in

@Thickness 0.125 in
ASTM D955
Oxford Polymers PC 714-FR Series PC, Flame retardant
Product Description: Amorphous, Polycarbonate injection molding grade, flame retardant Processing and Delivery Form: Pellets and Injection MoldingAdditives: Release Agents and UV stabilizersSpecial..
Linear Mold Shrinkage, Flow 0.00500 - 0.00700 cm/cm

@Thickness 3.17 mm
0.00500 - 0.00700 in/in

@Thickness 0.125 in
ASTM D955
Oxford Polymers PEI 1000 PEI
Product Description: (Unreinforced), Polyetherimide injection molding grade Processing and Delivery Form: Pellets and Injection Molding Special Characteristics: Colors AvailableInformation provided..
Linear Mold Shrinkage, Flow 0.00500 - 0.00700 cm/cm
0.00500 - 0.00700 in/in
Injection and Compression; ISO 2577
Raschig Group EPOXIDUR® 3581 S ZC EP Epoxy Molding Compound
Inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very good sealing connection on ..
Linear Mold Shrinkage, Flow 0.00400 - 0.00700 cm/cm
0.00400 - 0.00700 in/in
Compression; ISO 2577
Raschig Group RALUPOL® 4802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
Linear Mold Shrinkage, Flow 0.00500 - 0.00700 cm/cm

@Thickness 3.17 mm
0.00500 - 0.00700 in/in

@Thickness 0.125 in
ASTM D955
Oxford Polymers PC C20-000 Clear PC
Product Description: Amorphous, Unreinforced Polycarbonate injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Pigment onlySpecial Characteristics: Easy fl..
Linear Mold Shrinkage, Flow 0.00500 - 0.00700 cm/cm

@Thickness 3.17 mm
0.00500 - 0.00700 in/in

@Thickness 0.125 in
ASTM D955
Oxford Polymers PC/ABS 604i-FR PC/ABS, Flame retardant
Product Description: Amorphous, Polycarbonate & ABS, Flame retardant, Injection Molding Grade, VO rated @ 3.0mm. V2 rated @ 1.5mm Processing and Delivery Form: Pellets and Injection MoldingAdditive..
Linear Mold Shrinkage, Flow 0.00500 - 0.00700 cm/cm

@Thickness 3.17 mm
0.00500 - 0.00700 in/in

@Thickness 0.125 in
ASTM D955
Oxford Polymers PEI 1010 PEI
Product Description: (Unreinforced), Polyetherimide injection molding grade, high flow Processing and Delivery Form: Pellets and Injection Molding Additives: Release AgentsSpecial Characteristics: ..
Linear Mold Shrinkage, Flow 0.00400 - 0.00700 cm/cm
0.00400 - 0.00700 in/in
Compression; ISO 2577
Raschig Group RALUPOL® 802 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength, good heat resistance. This product meets the allowed up..
Linear Mold Shrinkage, Flow 0.00400 - 0.00700 cm/cm
0.00400 - 0.00700 in/in
Compression; ISO 2577
Raschig Group RALUPOL® 804 UP Polyester
Glass-fiber reinforced polyester molding compound. Low molding shrinkage and post-shrinkage, good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy m..