Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0046 cm/cm @Time 86400 sec |
0.0046 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 LNP* Konduit* PX08321 a compound based on PA6 resins containing mineral. Added features include: Thermally Conductive. |
|||
Linear Mold Shrinkage, Flow | 0.0046 cm/cm @Time 86400 sec |
0.0046 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP KONDUIT PX08321 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 compound |
|||
Linear Mold Shrinkage, Flow | 0.0046 cm/cm | 0.0046 in/in | |
Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product of.. |
|||
Linear Mold Shrinkage, Flow | 0.0046 cm/cm | 0.0046 in/in | SABIC Method |
SABIC Innovative Plastics ULTEM SF2250 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
Linear Mold Shrinkage, Flow | 0.0046 cm/cm | 0.0046 in/in | SABIC Method |
SABIC Innovative Plastics Ultem SF2250 PEI Blend (Europe-Africa-Middle East) High flow Ultem for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.0046 cm/cm | 0.0046 in/in | SABIC Method |
SABIC Innovative Plastics ULTEM SF2260 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
Linear Mold Shrinkage, Flow | 0.0046 cm/cm | 0.0046 in/in | SABIC Method |
SABIC Innovative Plastics ULTEM SF2250 PEI Blend High flow Ultem for thin wall application |
|||
Linear Mold Shrinkage, Flow | 0.0046 cm/cm | 0.0046 in/in | Sheet |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Linear Mold Shrinkage, Flow | 0.0046 cm/cm | 0.0046 in/in | 60x60x2 mm; ISO 294 |
BASF Ultradur® S 4090 G4X 20% Glass Filled PBT Description: Is a PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 20% of glass fibers for industrial parts with high dimensional stab.. |