Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0027 cm/cm
0.0027 in/in
ISO 294-4, 2577
Lanxess Durethan® DP BKV 240 H2.0 901510 Copolyamide, 40% Glass Fiber
CoPA, injection molding grade, 40% glass fibers reinforced, elastomer-modified, good heat-ageing resistance
Linear Mold Shrinkage, Flow 0.0027 cm/cm
0.0027 in/in
ISO 294-4, 2577
Lanxess Durethan® BKV 30 G H2.0 900051 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance, good UV s..
Linear Mold Shrinkage, Flow 0.0027 cm/cm
0.0027 in/in
ISO 294-4, 2577
Lanxess Durethan® BKV 30 G H2.0 900116 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance
Linear Mold Shrinkage, Flow 0.0027 cm/cm
0.0027 in/in
TM=320°C, TW=100°C
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Conditioned)
Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°..
Linear Mold Shrinkage, Flow 0.0027 cm/cm
0.0027 in/in
TM=320°C, TW=100°C
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry)
Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°..
Linear Mold Shrinkage, Flow 0.0027 cm/cm
0.0027 in/in
60x60x2 mm; ISO 294
BASF Ultradur® S 4090 G6 High Speed 30% Glass Filled PBT
Description: Is a PBT + ASA, easy-flowing injection-molding grades with 30% glass fibers; for rigid, tough and dimensionally stable technical parts.Applications: Housings, consoles, contact carriers..