Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0012 cm/cm
0.0012 in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber
PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
Linear Mold Shrinkage, Flow 0.0012 cm/cm

@Thickness 3.17 mm
0.0012 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Elastoblend® PA6 GF30 IM HS L 30% Glass Filled (Conditioned)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI..
Linear Mold Shrinkage, Flow 0.0012 cm/cm

@Thickness 3.17 mm
0.0012 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Elastoblend® PA6 GF30 IM HS L 30% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Impact Modifier Features: Impact ModifiedProcessing Method: Injection MoldingI..
Linear Mold Shrinkage, Flow 0.0012 - 0.0022 cm/cm

@Thickness 3.20 mm
0.0012 - 0.0022 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics ULTEM UC1200 PEI (Asia Pacific)
12% carbon fiber reinforced Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 listing in recognized colors.
Linear Mold Shrinkage, Flow 0.0012 cm/cm
0.0012 in/in
ISO 294-4
Solvay Specialty Polymers Kalix® 9945 HFFR Polyamide, High Performance (HPPA), 45% Glass Fiber
Kalix® 9945 HFFR is a 45% glass-fiber reinforced, halogen-free flame retardant High Performance Polyamide. It is hot-water moldable and intended for use in components requiring superior mechanica..
Linear Mold Shrinkage, Flow 0.0012 cm/cm

@Thickness 3.17 mm
0.0012 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® PA4/6 CF40 IM HS 40% Carbon Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites..
Linear Mold Shrinkage, Flow 0.0012 - 0.0022 cm/cm

@Thickness 3.20 mm
0.0012 - 0.0022 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI
LNP* Stat-kon* Ultem_UC1200 is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications.
Linear Mold Shrinkage, Flow 0.0012 - 0.0022 cm/cm

@Thickness 3.20 mm
0.0012 - 0.0022 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON Ultem_UC1200 PEI (Europe-Africa-Middle East)
LNP* Stat-kon* Ultem_UC1200 compound is a 12% carbon fiber reinforced PEI. High modulus with ESD characteristics for high-heat applications.
Linear Mold Shrinkage, Flow 0.0012 cm/cm

@Thickness 3.17 mm
0.0012 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® PA6/6 GF6 L BK 6% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 6% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackInformation provided by TP Comp..
Linear Mold Shrinkage, Flow 0.0012 cm/cm

@Thickness 3.17 mm
0.0012 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® PEEK HF
Availability: North AmericaForms: PelletsFeatures: Low ViscosityInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.0012 cm/cm

@Thickness 3.20 mm
0.0012 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP 9X10312 PA (Asia Pacific)
9X10312 is 50% glass fiber reinforced, impact modified nylon material. High modulus, high flow and good ductility, Low Moisture Absorption.
Linear Mold Shrinkage, Flow 0.0012 cm/cm
0.0012 in/in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP AF006 ABS (Europe-Africa-Middle East)
LNP* Thermocomp* AF006 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber.
Linear Mold Shrinkage, Flow 0.0012 cm/cm
0.0012 in/in
GB/T 15585-1995
Sichuan Deyang Haton® hCF31 Polyphenylene Sulfide
Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD
Linear Mold Shrinkage, Flow 0.0012 cm/cm

@Thickness 3.20 mm
0.0012 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Flow 0.0012 cm/cm
0.0012 in/in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP MF006A PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MF006A is a compound based on Polypropylene resin containing Glass Fiber.
Linear Mold Shrinkage, Flow 0.0012 cm/cm

@Thickness 3.20 mm
0.0012 in/in

@Thickness 0.126 in
ASTM D955
Samsung Cheil Industries Infino® NH-1150HH PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Linear Mold Shrinkage, Flow 0.0012 cm/cm

@Thickness 3.17 mm
0.0012 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES HiFill® PA4/6 CF40 IM HS 40% Carbon Filled (Conditioned)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites..
Linear Mold Shrinkage, Flow 0.0012 cm/cm
0.0012 in/in
GB/T 15585-1995
Sichuan Deyang Haton® hMR61LC1 Polyphenylene Sulfide, Glass & Mineral Reinforced
Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD
Linear Mold Shrinkage, Flow 0.0012 cm/cm
0.0012 in/in
SABIC Method
SABIC Innovative Plastics LNP STAT-KON KX97157 Acetal Copolymer (Europe-Africa-Middle East)
LNP* STATKON* KX97157 is a compound based on Acetal resin containing Carbon. Added features include : Electrically Conductive, Impact Modified.
Copyright © lookpolymers.com All Rights Reserved