Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.04572 cm/cm | 0.04572 in/in | 1/8" bar |
BASF Ultramid® BU50I BK 106 PA6 (Conditioned) Description: Ultramid Ultratough Nylon BU50I BK-106 is an unreinforced PA6, impact modified, pigmented black, injection molding product that maintains its impact strength and ductility to -40 deg F .. |
|||
Linear Mold Shrinkage | 0.04572 cm/cm | 0.04572 in/in | 1/8" bar |
BASF Ultramid® BU50I BK 106 PA6 (Dry) Description: Ultramid Ultratough Nylon BU50I BK-106 is an unreinforced PA6, impact modified, pigmented black, injection molding product that maintains its impact strength and ductility to -40 deg F .. |
|||
Linear Mold Shrinkage | 0.04572 cm/cm | 0.04572 in/in | 1/8" bar |
BASF Ultramid® BU50I PA6 (Conditioned) Description: Ultramid Ultratough Nylon BU50I is an unreinforced PA6, impact modified injection molding product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme .. |
|||
Linear Mold Shrinkage | 0.04572 cm/cm | 0.04572 in/in | 1/8" bar |
BASF Ultramid® BU50I PA6 (Dry) Description: Ultramid Ultratough Nylon BU50I is an unreinforced PA6, impact modified injection molding product that maintains its impact strength and ductility to -40 deg F (-40 deg C). The extreme .. |