Linear Mold Shrinkage 0.020 - 0.040 cm/cm
0.020 - 0.040 in/in
Multibase TPSiV® 4000-50A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; UV stableAPPLICATIONS: Solution for soft touch overmolding on consumer electronics, mob..
Linear Mold Shrinkage 0.020 - 0.040 cm/cm
0.020 - 0.040 in/in
Multibase TPSiV® 4200-50A Thermoplastic Elastomer
FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e..
Linear Mold Shrinkage 0.030 - 0.040 cm/cm
0.030 - 0.040 in/in
Daikin NEOFLON EA-LR43 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Linear Mold Shrinkage 0.030 - 0.040 cm/cm
0.030 - 0.040 in/in
Daikin NEOFLON EP-521 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Linear Mold Shrinkage 0.030 - 0.040 cm/cm
0.030 - 0.040 in/in
Daikin NEOFLON EP-610 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Linear Mold Shrinkage 0.030 - 0.040 cm/cm
0.030 - 0.040 in/in
Daikin NEOFLON EP-610AS ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Linear Mold Shrinkage 0.030 - 0.040 cm/cm
0.030 - 0.040 in/in
Daikin NEOFLON RP-4020 EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
Linear Mold Shrinkage 0.030 - 0.040 cm/cm
0.030 - 0.040 in/in
Daikin NEOFLON RP-4040 EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
Linear Mold Shrinkage 0.030 - 0.040 cm/cm
0.030 - 0.040 in/in
Daikin NEOFLON RP-5000 EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
Linear Mold Shrinkage 0.030 - 0.040 cm/cm
0.030 - 0.040 in/in
Daikin NEOFLON RP-5000AS EFEP Pellets
NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop..
Linear Mold Shrinkage 0.030 - 0.040 cm/cm
0.030 - 0.040 in/in
Daikin NEOFLON EP-620 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..
Linear Mold Shrinkage 0.030 - 0.040 cm/cm
0.030 - 0.040 in/in
Daikin NEOFLON EP-541 ETFE Pellets
Due to its excellent melt flow properties, NEOFLON ETFE can be processed in the same was as other thermoplastic resins. NEOFLON ETFE is also highly suited to such secondary processes as welding, fl..