Polymer Property : Linear Mold Shrinkage = 0.031 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.031 cm/cm
0.031 in/in
Radial shrinkage of 10 cm o.d. sintered rod at 23°C
Solvay Specialty Polymers Algoflon® F 5/S Polytetrafluoroethylene (PTFE)
Algoflon® F 5/S is a fine cut homopolymer PTFE powder that is white, granular and non-free flowing powder. It is designed for compounds production and in particular it is recommended for use with..
Linear Mold Shrinkage 0.031 cm/cm
0.031 in/in
ASTM D955
Teknor Apex Monprene® MP-2290A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Linear Mold Shrinkage 0.031 cm/cm
0.031 in/in
Radial shrinkage of 10 cm o.d. sintered rod at 23°C
Solvay Specialty Polymers Algoflon® F6 PTFE (Polytetrafluoroethylene)  (discontinued **)
Data provided by the manufacturer.Type II Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high inertness, excellent dielectric prope..