Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.018 - 0.028 cm/cm | 0.018 - 0.028 in/in | ISO DIS 294-4 |
Wellman Wellamid® GS1791-N2 5% Glass Sphere Reinforced, Natural Nylon 66 Description: Glass Sphere Reinforced, Natural Nylon 66Information provided by Wellman. |