Polymer Property : Linear Mold Shrinkage = 0.0237 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0237 cm/cm
0.0237 in/in
STN 64 0808
Plastcom SLOVALEN PC 78 FRD 3 Polypropylene Copolymer, Halogen Flame Retardant
FeaturesDetermined for environment where contact with water is possible because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machine..