Polymer Property : Linear Mold Shrinkage = 0.0092 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0092 cm/cm
0.0092 in/in
ASTM D955
North Wood Plastics 60 PP + UNIFILL (20% Wood Fiber)
Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It..
Linear Mold Shrinkage 0.0092 cm/cm
0.0092 in/in
STN 64 0808
Plastcom SLOVASTER® B GF 20 FRL 4 Polybutylene Terephthalate, 20% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant
FeaturesPBT with the content of 20% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth..