Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0092 cm/cm | 0.0092 in/in | ASTM D955 |
North Wood Plastics 60 PP + UNIFILL (20% Wood Fiber) Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It.. |
|||
Linear Mold Shrinkage | 0.0092 cm/cm | 0.0092 in/in | STN 64 0808 |
Plastcom SLOVASTER® B GF 20 FRL 4 Polybutylene Terephthalate, 20% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant FeaturesPBT with the content of 20% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth.. |