Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | ASTM D955 |
Multibase Multi-Pro® 3018 TU Polypropylene Talc Filled, 30% by weight.Forms:PelletsProcessing Methods:Injection MoldingUses: Automotive Under the HoodInformation provided by Multibase |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | ASTM D955 |
RheTech Products FT7011-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Claddings and faciasExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | STN 64 0808 |
Plastcom SLOVASTER® B GF 20 Polybutylene Terephthalate, 20% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 20% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | |
Plastcom SLOVASTER® B1 GF 20 PBT, 20% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | |
Plastcom SLOVASTER® B1 HML GF 20 PBT, 20% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 NG GF 30 Polyamide 6, 30% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 30% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | |
Plastcom SLOVAMID 6 T 30 TS PA6, 30% mineral filling FeaturesDecreased shrinkage against the BT types, increased heat application. Increased modulus in tension - strength of the material. PA matrix reduction. PA for injection moulding with the content.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | |
Plastcom SLOVASTER® B GB 20 M PBT, 20% glass beads FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | ASTM D955 |
RheTech Products HP511-00 27% Talc Reinforced Polypropylene Copolymer, High Performance, Non-UV Stabilized, Natural Applications: Interior trimCenter consolesI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | |
Huntsman IROGRAN® A 80 H 4826 TPU-Polyester Introduction: IROGRAN A 80 H 4826 is a thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of this product are excellent mechanical properties and hig.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | Isotropy |
Solvay TECHNYL® A 230 V13 PA66, 13% glass fiber, DRY Description: Modified polyamide 66, reinforced with 13% of glass fiber, with improved impact resistance, for injection molding.Available in: Europe and North AmericaProduct Applications: In addition.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | Isotropy |
Solvay TECHNYL® A 238 V13 PA66, 13% glass fiber, DRY Description: Polyamide 66, reinforced with 13% of glass fiber, heat stabilized, with improved impact resistance, for injection molding.Available in: Europe, Latin America and North AmericaProduct Ap.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | ASTM D955 |
Sumitomo Bakelite Durez® 25378 Phenolic, Injection Grade Durez 25378 Black Phenolic is a two stage heat resistant/electrical grade molding material having an excellent molded finish, low shrinkage and good heat resistance. Durez 25378 has exceptional UL .. |
|||
Linear Mold Shrinkage | 0.0085 - 0.0095 cm/cm | 0.0085 - 0.0095 in/in | Borealis Method |
Borealis Daplen™ EE115T TPO Compound Daplen EE115T is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE115T is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | ASTM D955 |
Plenco 7100 Phenolic, Nodular, Injection Molded PLENCO 07100 is an organic fiber reinforced phenolic molding compound, with improved mechanical strength properties and an industrial finish. 07100 is densified for easy handling and good pourabilit.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | ASTM D955 |
Tipco Tipcolene® CR 6216 - 40% Talc/Mineral Reinforced Polypropylene Copolymer Compound with Controlled Rheology 40% Mineral Reinforced, Controlled Rheology PP CopolymerApplications: Automotive Air DuctsProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Linear Mold Shrinkage | 0.0085 - 0.0095 cm/cm | 0.0085 - 0.0095 in/in | Borealis Method |
Borealis Daplen™ EE015U TPO Compound Daplen EE015U is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE015U is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | Bayer Test |
Covestro Bayflex® XGT-100 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | Bayer Test |
Covestro Bayflex® XGT-140 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | Bayer Test |
Covestro Bayflex® XGT-16 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | Bayer Test |
Covestro Bayflex® XGT-50 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | Bayer Test |
Covestro Bayflex® XGT-80 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | Injection; ASTM D955 |
Chang Chun Plastic Longlite PM T376J Heat Resistant Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | restricted |
BASF Ultramid® A3K BK 00464 PA66 (Conditioned) Description: Easy flowing injection-molding grade for fast processing. Uses include highly stressed technical parts such as bearings and gear wheels; also electrically insulating parts such as termi.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | restricted |
BASF Ultramid® A3W PA66 (Conditioned) Description: Free-flowing, heat aging resistant and rapidly processable grade for technical parts subject to high stress such as bearings and bearing cages, gearwheels and spool bodies.Information p.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | restricted |
BASF Ultramid® A3Z BK 30464 PA66 (Conditioned) Description: Impact-modified and stabilized injection- molding grade for components and housings with good low temperature impact resistance.Information provided by BASF |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 T 30 Polyamide 6, 30% Micronized Talc FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | mold average;Borealis Method |
Borealis Daplen™ EF103AE Polypropylene TPO Compound Daplen™ EF103AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, high melt flow rate an.. |
|||
Linear Mold Shrinkage | 0.0085 cm/cm | 0.0085 in/in | |
Plastcom SLOVAMID 6 NG GF 30 LS PA6, 30% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 30% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |