Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0072 cm/cm | 0.0072 in/in | |
Plastcom SLOVALEN PH 49 GF 25 PP, 25% glass fibre, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 25 % glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP.. |
|||
Linear Mold Shrinkage | 0.0072 cm/cm | 0.0072 in/in | |
Plastcom SLOVALEN PH 59 GF 30 PP, 30% glass fibre FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suita.. |
|||
Linear Mold Shrinkage | 0.0072 cm/cm | 0.0072 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 GF 25 FRA 5 Polyamide 6, 25% Glass Fiber, Halogen Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,.. |
|||
Linear Mold Shrinkage | 0.0072 cm/cm | 0.0072 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 GF 30 FRG 5 Polyamide 6, 30% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,.. |
|||
Linear Mold Shrinkage | 0.0072 cm/cm | 0.0072 in/in | ASTM D955 |
North Wood Plastics HDPE with 40% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Linear Mold Shrinkage | 0.0072 cm/cm | 0.0072 in/in | |
Plastcom SLOVAMID 6 GF 25 FRA 5 LS PA6, 25% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 25% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,.. |
|||
Linear Mold Shrinkage | 0.0072 cm/cm | 0.0072 in/in | Isotropy |
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ.. |
|||
Linear Mold Shrinkage | 0.0072 cm/cm | 0.0072 in/in | ASTM D955 |
Plenco 7591 Phenolic, Briquette, Injection Molded PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |