Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0057 cm/cm | 0.0057 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 GF 15 Polyamide 6, 15% Glass Fiber FeaturesPA 6 for injection moulding, chemically reinforced with 15% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and .. |
|||
Linear Mold Shrinkage | 0.0057 cm/cm | 0.0057 in/in | Isotropy |
Solvay TECHNYL® A 218 V40 PA66, 40% glass fiber, DRY Description: Polyamide PA66, reinforced with 40% of glass fiber, heat stabilized for injection molding.Available in: Asia Pacific, Europe and North AmericaProduct Applications: TECHNYL A 218 V40 is .. |
|||
Linear Mold Shrinkage | 0.0057 cm/cm | 0.0057 in/in | Isotropy |
Solvay TECHNYL® A 218 V43 Black 21 N PA66, 43% glass fiber, DRY Description: Polyamide PA66, reinforced with 43% of glass fiber, heat stabilized, for injection molding.Available in: North AmericaProduct Applications: TECHNYL® A 218 V43 is used in all sectors .. |
|||
Linear Mold Shrinkage | 0.0057 cm/cm | 0.0057 in/in | Isotropy |
Solvay TECHNYL® C 218 MZ20 V10 Black Z PA6, 20/10% mineral/glass fiber, DRY Description: Polyamide PA6, reinforced 20 % mineral filler and 10 % of glass fiber, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL C 218 MZ20 V10 offe.. |
|||
Linear Mold Shrinkage | 0.0057 cm/cm | 0.0057 in/in | Isotropy |
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized.. |
|||
Linear Mold Shrinkage | 0.0057 cm/cm | 0.0057 in/in | ASTM D955 |
Plenco 00757 Melamine-Phenolic, Granular, Injection Molded PLENCO 00757 is a melamine-phenolic, copolymer molding compound, offering excellent arc resistance and comparative track index values. It is formulated to provide improved mechanical strength proper.. |
|||
Linear Mold Shrinkage | 0.0057 cm/cm | 0.0057 in/in | ASTM D955 |
Plenco 2482 Phenolic, Granular, Transfer Molded PLENCO 02482 is a general purpose, organic filled phenolic molding compound offering excellent mechanical strength while maintaining dielectric properties at elevated humidity levels. UL recognized .. |
|||
Linear Mold Shrinkage | 0.0057 cm/cm | 0.0057 in/in | ASTM D955 |
Plenco 7591 Phenolic, Pellet, Transfer Molded PLENCO 07591 is a mineral and flock cotton filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco. |