Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0045 - 0.0055 cm/cm
0.0045 - 0.0055 in/in
ASTM D955
PolyOne Edgetek® PF-05GF/000 Polysulfone, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Linear Mold Shrinkage 0.0045 - 0.0055 cm/cm
0.0045 - 0.0055 in/in
Polyram PlusTek PA301G3 Nylon 6.6, Heat Stabilized, 15% Glass Fiber
Heat stabilized, 15% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0045 - 0.0055 cm/cm
0.0045 - 0.0055 in/in
Injection Molding; ISO 2577
Vyncolit 3640 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..
Linear Mold Shrinkage 0.0045 - 0.0055 cm/cm
0.0045 - 0.0055 in/in
Polyram PlusTek RA303G4 Nylon 6.6, 20% Glass Fiber
20% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0045 - 0.0055 cm/cm
0.0045 - 0.0055 in/in
Polyram PlusTek RA307G4 Nylon 6.6, 20% Glass Fiber
20% glass fiber reinforced heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0050 - 0.0055 cm/cm
0.0050 - 0.0055 in/in
Annealed; ASTM D955
Dow DT702 TPO
Dow Fascia TPO for Painted ApplicationsInformation provided by Dow
Linear Mold Shrinkage 0.0045 - 0.0055 cm/cm
0.0045 - 0.0055 in/in
IS 13411-1992
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded
Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg..
Linear Mold Shrinkage 0.0035 - 0.0055 cm/cm
0.0035 - 0.0055 in/in
IS 13411-1992
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded
Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R..
Linear Mold Shrinkage 0.0035 - 0.0055 cm/cm
0.0035 - 0.0055 in/in
IS 13411-1992
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded
Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R..
Linear Mold Shrinkage 0.0030 - 0.0055 cm/cm
0.0030 - 0.0055 in/in
Bulk Molding Compounds BMC 700 Thermoset Polyester, High Arc Quench Electrical Grade
BMC 700 is a general purpose, mineral filled, glass fiber-reinforced polyester compound that was initially designed for molding arc chutes. It has superior arc quench properties. As with all other B..
Linear Mold Shrinkage 0.0050 - 0.0055 cm/cm
0.0050 - 0.0055 in/in
ASTM D955
PolyOne Edgetek® NL-10GF/000 Nylon 6/12, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedInformation provided by PolyOne Corporation.
Linear Mold Shrinkage 0.0050 - 0.0055 cm/cm
0.0050 - 0.0055 in/in
ASTM D955
PolyOne Edgetek® AT-25GF/000 Acetal-Copolymer, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Linear Mold Shrinkage 0.0045 - 0.0055 cm/cm
0.0045 - 0.0055 in/in
ISO 2577
Polyram PlusTek RA325G4 Nylon 66 for Injection Molding, 20% Glass-Fiber Reinforced, Self-Extinguishing, Halogen Free
20% Glass-fiber reinforced, self-extinguishing halogen free Nylon 66 for injection molding applications.Information provided by Polyram.
Linear Mold Shrinkage 0.0050 - 0.0055 cm/cm
0.0050 - 0.0055 in/in
ASTM D955
PolyOne Edgetek® SF-10GF/000 Polyphenylene Sulfide (PPS), Glass Filled  (discontinued **)