Polymer Property : Linear Mold Shrinkage = 0.00250 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.000600 - 0.00250 cm/cm
0.000600 - 0.00250 in/in
Average value: 0.00138 cm/cm Grade Count:5
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is..