Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00075 cm/cm | 0.00075 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1281-47 VE SMC Description: Premi-Glas® 1281-47 VE is a sheet molding compound.Market: StructuralInformation provided by Premix. |
|||
Linear Mold Shrinkage | 0.00075 cm/cm | 0.00075 in/in | |
Haysite 14100 Polyester BMC, 15% Glass Reinforced The 14100 series bulk molding compound is an electrical grade material that can be compression, transfer, or injection molded. Offering good mechanical strength and excellent electrical properties, .. |