Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00040 cm/cm | 0.00040 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1205 Glass Reinforced SMC Description: Premi-Glas® 1205 is a glass reinforced thermoset Sheet Molding Compound formulated for residential door skins and similar construction applications. Key features and benefits: Excellen.. |
|||
Linear Mold Shrinkage | 0.00040 cm/cm | 0.00040 in/in | Polymerization Shrinkage |
Premix Premi-Glas® 1261-28 VE Glass Reinforced Vinyl Ester TMC Description: Premi-Glas® 1261-28 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Excellent thermal stability an.. |
|||
Linear Mold Shrinkage | 0.00040 cm/cm | 0.00040 in/in | |
Network Polymers Softflex® 1104 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Linear Mold Shrinkage | 0.00040 - 0.0020 cm/cm | 0.00040 - 0.0020 in/in | ASTM D955 |
IDI Composites 46-3 Thermoset Polyester, Molding Superior electrical performance with low pressure molding for V-O flammability in encapsulation applications.Data provided by the manufacturer. |
|||
Linear Mold Shrinkage | 0.00040 cm/cm | 0.00040 in/in | ISO 2577 |
Menzolit Menzolit® SMC 1100 Unsaturated Polyester UP SMC 1100 is a special vinylester SMC for high strength applications. The reinforcement has been put to a level that combines mouldability with high strength and stiffness properties. The specific re.. |
|||
Linear Mold Shrinkage | 0.00040 cm/cm | 0.00040 in/in | |
Lucite International Series 100 Liquid Acrylic Resin LUCITE® LIQUID ACRYLIC RESINS SERIES 100For the manufacture of solid surface shapesAmbient temperature cureCan be used on batch or continuous in-line mixing equipmentInformation provided by Lucit.. |
|||
Linear Mold Shrinkage | 0.00040 cm/cm | 0.00040 in/in | per ATM D955. Post shrinkage is 0.04% at 72hr 120ºC per ASTM D1299. |
Plenco 6553 Phenolic, Granular, Compression Molded Two-Stage Phenolic. PLENCO 06553 is a phenolic molding compound, formulated specifically for automotive brake pistons. 06553 exhibits excellent dimensional stability, and resistance to brake fluids.. |
|||
Linear Mold Shrinkage | 0.00040 cm/cm | 0.00040 in/in | flex bar; ASTM D955 |
Lubrizol ESTALOC® 59300 Polyester-Type, Reinforced Engineering Thermoplastic Polyurethane Features: Fast Cycling, Dimensional Stability, Durability, Aesthetics, Low Temperature ImpactUses: Injection MoldingAvailability: Americas, Europe, Middle East, Africa, India and AsiaInformation pro.. |
|||
Linear Mold Shrinkage | 0.00040 cm/cm | 0.00040 in/in | ISO 2577 |
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound KINEL SK4502 S8 is a long carbon fiber reinforced BMI molding compound suited for very demanding tribological applications, high speeds and temperatures even under dry running conditions. Thermal ex.. |
|||
Linear Mold Shrinkage | 0.00040 cm/cm | 0.00040 in/in | |
Lucite International Series 500 Liquid Acrylic Resin LUCITE® LIQUID ACRYLIC RESINS SERIES 500For the manufacture of solid surface sheet & worktopsAmbient temperature curing resin with low VOC emissionsCan be used on batch or continuous in-line mixing.. |