Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.00030 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
Polymerization Shrinkage
Premix Premi-Glas® 3404 33% Glass Reinforced SMC
Description: Premi-Glas® 3404 is a glass reinforced thermoset sheet molding compound designed for mass transit and high strength flame retardant applications where low smoke and flame are required...
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
Polymerization Shrinkage
Premix Premi-Glas® 8101 Glass Reinforced Polyester BMC
Description: Premi-Glas® 8101 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex..
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
ISO 2577
Menzolit Menzolit® BMC 1100 Unsaturated Polyester UP
BMC 1100 is a special BMC for high strength application. The glass content is set to a level that provides sufficient mouldability with high strength and stiffness properties. The selection of the r..
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
ISO 2577
Menzolit Menzolit® BMC 1500 Unsaturated Polyester UP
BMC 1500 is a special BMC for the use at elevated temperature. The glass content is set to a level that combines good flowability with good strength and stiffness properties. Even without a specific..
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
ISO 2577
Menzolit Menzolit® SMC 0520 Unsaturated Polyester UP
SMC 0520 is a special SMC with significantly reduced density. The glass level has been selected to combine good moulding with sufficient strength and stiffness properties. Even without a specific fi..
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
ISO 2577
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP
SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc..
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
ISO 2577
Menzolit Menzolit® BMC 1400 Unsaturated Polyester UP
BMC 1400 is a special BMC for the use on an engine. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The product has been developped f..
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
ASTM D955
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate
Information provided by A. Schulman.
Linear Mold Shrinkage 0.00030 cm/cm

@Thickness 1.59 mm
0.00030 in/in

@Thickness 0.0625 in
ASTM D955
Plastics Group Polifil® GFRMPPCC-40 40% Glass Reinforced Polypropylene, High Impact
Polifil® GFRMPPCC series compounds are high impact polypropylenes reinforced with chemically coupled glass fibers. This combination provides higher impact strength while retaining high stiffness.Ap..
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
ASTM D955
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate
Information provided by A. Schulman.
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
ASTM D955
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate
Information provided by A. Schulman.
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
ASTM D955
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate
Information provided by A. Schulman.
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
ASTM D955
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate
Information provided by A. Schulman.
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
ASTM D955
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate
Information provided by A. Schulman.
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
Cured
Atom Adhesives AA-DUCT 902 Epoxy Adhesive and Coating
AA-DUCT 902 is an epoxy adhesive and coating formulation based on pure silver. This versatile silver formulation offers the maximum continuity of conductivity with an electrical resistivity value of..
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
ASTM D2566
BCC Products BC 8782 Urethane Casting
BC 8782 produces a high impact rigid 82 Shore D material that is commonly used to make clear or tinted castings of all kinds. When used at room temperature castings 1/8" thick or larger can be readi..
Linear Mold Shrinkage 0.00030 cm/cm
0.00030 in/in
Polyram Polytron P50B01 Homopolymer Polypropylene, Chemically Coupled 50% LGF
A chemically coupled 50% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.00030 - 0.0010 cm/cm
0.00030 - 0.0010 in/in
Bulk Molding Compounds BMC T70 Automotive Grade Molding compound
BMC T70 is a low profile automotive grade molding compound specifically formulated for the vacuum metallization process. These compounds have excellent physical properties as well as superior adhes..
Copyright © lookpolymers.com All Rights Reserved