Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | -0.00200 - 0.00400 cm/cm | -0.00200 - 0.00400 in/in | Average value: 0.00159 cm/cm Grade Count:11 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Linear Mold Shrinkage | -0.00200 - 0.0010 cm/cm | -0.00200 - 0.0010 in/in | processing, expansion/shrinkage; ISO 2577 |
Bulk Molding Compounds tetra-DUR N 4203 Bulk Molding Compound Highest dimensional stability under temp. Low profile.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipat.. |