Polymer Property : Base Resin Melt Index = 2.5 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Base Resin Melt Index 2.5 g/10 min
2.5 g/10 min
ASTM D1238
Lotte Chemical Titan TITANEX® LF2554 Linear low density polyethylene Hexene-1 resin  (discontinued **)
LF2554 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for slot cast extrusion which offers outstanding toughness, extrudability and d..
Base Resin Melt Index 2.5 g/10 min
2.5 g/10 min
ASTM D1238
Eastman 184MF Polyethylene Film  (discontinued **)
Polyethylene 184MF is a low-density formulation with medium slip and low antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is character..
Base Resin Melt Index 2.5 g/10 min
2.5 g/10 min
ASTM D1238
Eastman 1925F Polyethylene Film  (discontinued **)
Polyethylene 1925F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require heat-sealing treated-to-treated film surfaces and where good..