Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Melt Index | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
Lotte Chemical Titan TITANEX® LF1041 Linear low density polyethylene resin
(discontinued **) LF1041 is a pelleted linear low density polyethylene resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown film extrusion which offers outstanding toughne.. |
|||
Base Resin Melt Index | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
Lotte Chemical Titan TITANEX® LF1043 Linear low density polyethylene resin
(discontinued **) LF1043 is a pelleted linear low density polyethylene resin formulated with antioxidant, and antiblock agent. This product is used for blown film extrusion which offers outstanding toughness, extrud.. |
|||
Base Resin Melt Index | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
Lotte Chemical Titan TITANEX® LF1044 Linear low density polyethylene resin
(discontinued **) LF1044 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and draw down.. |
|||
Base Resin Melt Index | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
Lotte Chemical Titan TITANEX® LF1051 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF1051 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant, high antiblock and slip agent. This product is used for blown film extrusion which offers outstandin.. |
|||
Base Resin Melt Index | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
Lotte Chemical Titan TITANEX® LF1054 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF1054 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and .. |
|||
Base Resin Melt Index | 1.0 g/10 min | 1.0 g/10 min | I<sub>2</sub>; ASTM D1238 |
Lotte Chemical Titan TITANCEED® mL1061 Linear low density polyethylene resin
(discontinued **) Titanceed® mL1061 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant, antiblock and slip agent. Films made from Titanceed® mL1061 have outstanding tensile.. |
|||
Base Resin Melt Index | 1.0 g/10 min | 1.0 g/10 min | I<sub>2</sub>; ASTM D1238 |
Lotte Chemical Titan TITANCEED® mL1064 Linear low density polyethylene resin
(discontinued **) Titanceed® mL1064 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL1064 have outstanding tensile, impact and puncture stre.. |
|||
Base Resin Melt Index | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
Westlake Hifor SC74561-F Clear (Voridian) Polyethylene Film, Using Energx Technology Services
(discontinued * VORIDIAN HIFOR CLEAR SC74558-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives. Films produced with t.. |
|||
Base Resin Melt Index | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
Lotte Chemical Titan TITANZEX® HM5001 High density polyethylene HM5001 is a high density polyethylene for yarn extrusion. HM5001 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 (c) 3.1a & 3.2aApplic.. |