Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Melt Index | 0.50 g/10 min | 0.50 g/10 min | ASTM D1238 |
Westlake Hifor LT74107-F Polyethylene Film, Using Energx Technology Services
(discontinued **) Hifor LT74107-F polymer is a high strength and good clarity polyethylene designed for blown film extrusion that contains medium slip, high antiblock and high processing aid additives. Films produced.. |