Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANEX® LF1044 Linear low density polyethylene resin
(discontinued **) LF1044 is a pelleted linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and draw down.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANEX® LF1054 Linear low density polyethylene Hexene-1 resin
(discontinued **) LF1054 is a pelleted linear low density polyethylene Hexene-1 resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding toughness, extrudability and .. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANEX® LI2516 Linear low density polyethylene resin
(discontinued **) LI2516 is a pelleted linear low density polyethylene with very narrow molecular weight distribution.Applications: House-wares, lids, closures and toys.Advantages: Excellent stress crack resistance,.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANCEED® mL1061 Linear low density polyethylene resin
(discontinued **) Titanceed® mL1061 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant, antiblock and slip agent. Films made from Titanceed® mL1061 have outstanding tensile.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANCEED® mL1064 Linear low density polyethylene resin
(discontinued **) Titanceed® mL1064 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL1064 have outstanding tensile, impact and puncture stre.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANCEED® mL156 Linear low density polyethylene resin
(discontinued **) Titanceed® mL156 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANCEED® mL216 Linear low density polyethylene resin
(discontinued **) Titanceed® mL216 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANCEED® mL2764 Linear low density polyethylene resin
(discontinued **) Titanceed® mL2764 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL2764 have outstanding tensile properties, impact streng.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lotte Chemical Titan TITANCEED® mL3564 Linear low density polyethylene resin
(discontinued **) Titanceed® mL3564 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL3564 have outstanding tensile properties, impact streng.. |
|||
Base Resin Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D4883 |
Eastman 1550F Film Polyethylene
(discontinued **) Polyethylene 1550F is a low density polyethylene that contains no additives.Eastman Chemical Company sold its polyethylene business to Westlake Chemical Corporation in Dec. 2006. This grade no long.. |