Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Antiblock Level = 3500 ppm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Antiblock Level 3500 ppm
3500 ppm
ExxonMobil LD 144.50 Packaging Film Resin
Film made from LD 144.50 offers improved impact strength and heat sealability compared to homopolymer clarity film resins. Typically applications include food packaging, frozen food packaging, and ..
Antiblock Level 3500 ppm
3500 ppm
ExxonMobil LL 1107x93 Blown Film Resin
Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr..
Antiblock Level 3500 ppm
3500 ppm
ExxonMobil LL 1107x95 Blown Film Resin
Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr..
Antiblock Level 3500 ppm
3500 ppm
ExxonMobil LLDPE LL 1002.80 Linear Low Density Polyethylene Resin
Product Description: LL 1002 resins are butane LLDPE designed for the blown film process. Films made form LL 1002 resins have very good tensile and toughness properties. LL 1002.09 is a granular mat..
Antiblock Level 3500 ppm
3500 ppm
ExxonMobil LLDPE LL 1107X93 Linear Low Density Polyethylene Resin
Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr..
Antiblock Level 3500 ppm
3500 ppm
ExxonMobil LLDPE LL 1107X95 Linear Low Density Polyethylene Resin
Product Description: LL 1107 resins are fractional melt index butane LLDPE blown film resins. Films made with LL 1107 resins have good stiffness and tensile strength. Theses resins’ strength and dr..
Antiblock Level 3500 ppm
3500 ppm
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe..
Antiblock Level 3500 ppm
3500 ppm
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Good Strength High Output Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7041 NT 7 is a half melt, ethylene-hexene copolymer, designe..
Copyright © lookpolymers.com All Rights Reserved