Polymer Property : Antiblock Level = 1245 ppm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Antiblock Level 1245 ppm
1245 ppm
Dow 611A Low Density Polyethylene (LDPE)
A shrink film resin with good optics packaging applications Optimum gauge range: 1.0 - 3.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow
Antiblock Level 1245 ppm
1245 ppm
Dow 611A Low Density Polyethylene (LDPE)
A shrink film resin with good optics packaging applications Optimum gauge range: 1.0 - 3.0 mil Complies with U.S. FDA 21 CFR 177.1520 (c) 2.1 Information provided by Dow