Polymer Property : Slip Level = 750 ppm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Slip Level 750 ppm
750 ppm
ExxonMobil LD 117.03 Blown Overwrap Film Resin  (discontinued **)
LD 117 resins are homopolymer film resins with good clarity and excellent stiffness. Film from LD 117 resins can be used in overwrap applications and push-through type packaging equipment. Film ma..
Slip Level 750 ppm
750 ppm
Additive - Erucamide
Borealis Himod™ FT7324 . LDPE for Film
Himod FT7324 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i..
Slip Level 750 ppm
750 ppm
Erucamide
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film
LDPE 1022 FH 24 is a low density polyethylene made by a high pressure process.LDPE 1022 FH 24 is a slip and anti-block formulated grade.LDPE 1022 FH 24 is suited to many applications in the field of..
Slip Level 750 ppm
750 ppm
Chevron Phillips MarFlex® 5335 Low Density Polyethylene, Blown Film
This LDPE is tailored for blown film applications that require:Good processabilityLow coefficient of frictionGood openabilityGood sealabilityTypical blown film applications include:Institutional pac..
Slip Level 750 ppm
750 ppm
ExxonMobil Exceed™ 2018EB Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 2018EB is a metallocene ethylene-hexene copolymer. The higher melt index makes this polymer ideally suited for blending into LDPE rich films. Availability: Africa & Middl..
Slip Level 750 ppm
750 ppm
ExxonMobil LD 105.BR Very High Clarity Packaging Film Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
Slip Level 750 ppm
750 ppm
ExxonMobil LD 143.26 High Clarity Packaging Film Resin
Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq..
Slip Level 750 ppm
750 ppm
ExxonMobil LDPE LD 100BR Low Density Polyethylene Resin
Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties..
Slip Level 750 ppm
750 ppm
ExxonMobil LDPE LD 104BR Low Density Polyethylene Resin
Product Description: LD 104BR is an LDPE grade, which offers good optical properties combined with increased stiffness.Availability: Africa & Middle East, Asia Pacific and Europe Additive: Antibloc..
Slip Level 750 ppm
750 ppm
ExxonMobil LDPE LD 105.BR Low Density Polyethylene Resin
Product Description: LD 105 resins are homopolymer packaging film resins designed for applications requiring outstanding clarity with good stiffness. These resins can be processed in either blown or..
Slip Level 750 ppm
750 ppm
ExxonMobil LDPE LD 136.MN Low Density Polyethylene Resin
Product Description: LD 136.MN is a homopolymer film resin with good clarity. The resin is suitable for processing on blown film equipmentAvailability: Latin America, North America and South America..
Slip Level 750 ppm
750 ppm
ExxonMobil LDPE LD 143.26 Low Density Polyethylene Resin
Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq..
Slip Level 750 ppm
750 ppm
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin
Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi..
Slip Level 750 ppm
750 ppm
ExxonMobil LDPE LD 362BR Low Density Polyethylene Resin
Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Slip Level 750 ppm
750 ppm
ExxonMobil LDPE LD 363BR Low Density Polyethylene Resin
Product Description: LD 363 series are LEVA LDPE grades, offering good optical and mechanical properties. Two additive combinations are available according to the required surface properties.Availab..
Slip Level 750 ppm
750 ppm
Dow AFFINITY™ PL 1881G Polyolefin Plastomer (POP)
AFFINITY™ PL 1881G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal products.In..
Slip Level 750 ppm
750 ppm
ExxonMobil Exceed™ 1018EB Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 1018EB is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018EB have outstanding tensile, impact, puncture resistance and low temperature properties. ..
Slip Level 750 ppm
750 ppm
ExxonMobil Exceed™ 2018EB Blown Film Resin  (discontinued **)
Exceed 2018EB resin is an ethylene based polymer produced with metallocene single site catalysts using ExxonMobil Chemicals Exxpol® Technology. The higher melt index makes this polymer ideally sui..
Slip Level 750 ppm
750 ppm
ExxonMobil Exceed™ 1018 EB Blown Film Resin  (discontinued **)
Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. ..