Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Molecular Weight = 7500 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 7500 g/mol
7500 g/mol
Westlake Epolene® E-20 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Product Description: Epolene E-20 is a medium density, low molecular-weight oxidized polyethylene with exceptional hardness and low color. It has a low softening point and low viscosity, which give ..
Molecular Weight 7500 g/mol
7500 g/mol
Westlake Epolene® EE-2 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer
Product Description: EE-2 is a medium density, low molecular-weight oxidized polyethylene with exceptional hardness. It is an excellent asphalt modifier which mixes readily with all asphalts. It h..