Physical Properties Metric English Comments
Molecular Weight 670 g/mol
670 g/mol
Mw; ETM 300-83
ExxonMobil ESCOREZ™ 5300 Petroleum Hydrocarbon Resin
The Escorez 5300 series resins are water white cycloaliphatic hydrocarbon resins. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, APP an d A..
Molecular Weight 670 g/mol
670 g/mol
Mw; ETM 300-83
ExxonMobil ESCOREZ™ 5400 Petroleum Hydrocarbon Resin
Light colored cycloaliphatic hydrocarbon resin. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, natural rubber, synthetic polyisoprene, poly..
Molecular Weight 670 g/mol
670 g/mol
3M Fluorinert™ FC-43 Electronic Liquid
3M™ Fluorinert™ Liquid FC-43 is a non-conductive, thermally and chemically stable liquid ideal for many single phase heat transfer fluid applications, especially in the electronics and semiconduct..