Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 6000 g/mol | 6000 g/mol | |
Dow VORANOL™ CP 6001 Polyol VORANOL™ CP 6001 polyol is a triol polyether polyol, capped, specially developed for the production flexible HR molded polyurethane foam with TDI, TDI/PMDI or MDI. It can be used in the production.. |
|||
Molecular Weight | 6000 g/mol | 6000 g/mol | |
BASF Pluracol® 220 Specialty Polyol Description: Pluracol® 220 polyol is a high molecular weight, primary hydroxyl terminated polyol used in polyurethane elastomer and sealant formulations.Information provided by BASF |
|||
Molecular Weight | 6000 g/mol | 6000 g/mol | |
Westlake Epolene® N-11 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-11 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |