Molecular Weight 419 g/mol
419 g/mol
LG Chemical DINP Plasticizer
Features: LG DINP is used cable and tarpaulin because it can reduce gas generation during operation due to low volatile compared to DOP.Application: Synthetic leather, sheet, power cableInformation ..