Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 4100 g/mol | 4100 g/mol | |
Solvay Specialty Polymers FOMBLIN® Y H-VAC 40/11 PFPE Pump Oil FOMBLIN Y fluids are a mixture of fluorinated polymers obtained by a photochemical process that begins with hexafluoropropylene. Since the FOMBLIN chemical chain contains only carbon, fluorine, and.. |
|||
Molecular Weight | 4100 g/mol | 4100 g/mol | |
Solvay Specialty Polymers FOMBLIN® Y45 PFPE Lubricant FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati.. |