Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 3200 g/mol | 3200 g/mol | |
Solvay Specialty Polymers FOMBLIN® Y25 PFPE Lubricant FOMBLIN Y perfluoropolyether fluids have the following unique features; excellent high temperature stability; good low temperature properties; very good E.P. and wear characteristics; good evaporati.. |